Neodymium Magnets
Ceramic Magnets
Samarium Cobalt Magnets
Alnico Magnets
Bonded Magnets
Magnetic Properties
For product technical information, pricing and availability contact our sales department at:
(219) 548-3799
sales@allianceorg.com

BCN - Bonded Compression Neo
BCNF - Bonded Neo Ferrite Hybrid
BIF - Bonded Injection Ferrite
BIN - Bonded Injection Neo
BIS - Bonded Injection SmCo
N - Sintered NdFeB
C - Sintered SrFe2O3 Ferrites
S - Sintered SmCo5, Sm2Co17
A - Cast and Sintered AlNiCo

SmCo S-28U

«« Back to Samarium Cobalt Magnetic Materials

S-28U properties
    Max Min
Residual Induction Br G 11,000 10,400
Coercive Force Hc Oe 10,500 9,500
Intrinsic Coercive Force Hci Oe 35,000 25,000
Max. Energy Product (BH)max MGOe 30 26
Material Density g/cm3 8.4
Max. Operating Temperature C 300
Temperature Coefficient for B %/C -0.03
Temperature Coefficient for H %/C -0.04
Required Magnetizing Force Oe 35,000
Material Composition Sm, Co, Cu, Zr, Pr

dotsSamarium Cobalt magnets have excellent temperature resistance to demagnetization and are used in high heat applications. Coating is not neccesary and tooling is not required.